In a carbon-in-pulp circuit, activated carbon is not only a reagent — it is a mechanical component, tumbled in slurry for months, screened, pumped, eluted at 130 °C and reactivated in a kiln. Every cycle grinds it. The gold that leaves the circuit adsorbed on carbon fines lost to tailings never appears on any invoice; it appears as a slow decline in the elution balance that most operations attribute to everything except the carbon.
Attrition loss has three paths, and only one is bought:
The lost fraction is fine carbon carrying its gold load into the tailings stream. At a pulp density of 15–25 g/L carbon, a carbon losing 5% of inventory per cycle versus one losing 2% writes the difference directly into the recovery ledger — at scale, it is the largest hidden cost in the circuit.
| Hardness (ball-pan) | Typical attrition loss per cycle | Annual make-up on 100 t inventory | Cost per ounce recovered |
|---|---|---|---|
| ≥97% | ~2% | Low | Lowest — despite unit price |
| 93–96% | ~3–4% | Moderate | Middle |
| ≤90% | ~5% + | High | Highest — gold to tailings |
Attrition figures are indicative for a well-run CIP circuit; kiln regime and slurry agitation move them materially. The direction of the relationship does not move at all.
The ball-pan abrasion test (the hardness number on the certificate) measures exactly this: a weighed sample tumbled with steel balls under defined conditions, and the percentage surviving the sieve. It is not a purity measure or a strength boast — it is a wear-rate proxy, and in carbon selection for gold duty it is the number that decides cost per ounce.
The arithmetic is blunt. Moving from a 90% hardness carbon to a 97% one roughly halves the fines generation rate per cycle. On a circuit carrying 100 tonnes of carbon inventory, that difference in annual make-up carbon alone typically exceeds the entire price premium of the harder product — before counting the gold it no longer carries to tailings.
Attrition never shows on the purchase order and always shows in the balance sheet. Reading hardness data properly — as a wear-rate prediction rather than a quality badge — is the cheapest optimisation available in a gold circuit.
Ten technical notes · no email gate
Spent carbon is a resource with a transport cost attached. A break-even calculation for thermal reactivation at different scales and distances.
Why acid-washed grades exist, what they remove, and when the extra cost is justified by the regulatory limit you must meet.
A jar test says whether carbon adsorbs. A column test says when the bed breaks through. How to run one that survives contact with the plant.
Iodine number measures micropores below 2 nanometres. It says almost nothing about decolourisation. Here is the number you should ask for instead.
Contaminant, inlet level, flow rate, target limit — four numbers are enough for a first recommendation and a media volume estimate.